Abstract

Wet-chemical approach is widely applied for phosphate recovery from incinerated ash of waste activated sludge (WAS), along with metals removed/recovered. The high contents of both aluminum (Al) and iron (Fe) in WAS-incinerated ash should be suitable for producing coagulants with some waste anions like Cl− and SO42− With acid (HCl) leaching and metals’ removing, approximately 88 wt% of phosphorus (P) in the ash could be recovered as hydroxylapatite (HAP: Ca5(PO4)3OH); Fe3+ in the acidic leachate could be selectively removed/recovered by extraction with an organic solvent of tributyl phosphate (TBP), and thus a FeCl3-based coagulant could be synthesized by stripping the raffinate with the original brine (containing abundant Cl− and SO42−). Furthermore, a liquid poly-aluminum chloride (PAC)-based coagulant could also be synthesized with Al3+ removed from the ash and the brine, which behaved almost the same in the coagulation performance as a commercial coagulant on both phosphate and turbidity removals. Both P-recovery from the ash and coagulant production associated with the brine would enlarge the markets of both ‘blue’ phosphate and ‘green’ coagulants.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call