Abstract

The combination of ball milling (BM), microwave irradiation (MI), and deep eutectic solvents (DES) results synergistic for an efficient, selective, and very rapid (10 min) delignification of materials with high lignin content (ca. 50 wt%) such as walnut shells (WS). Lignin is dissolved in the DES, whereas the polysaccharide fractions remain suspended with limited degradation, due to the rapid pretreatment. After ball milling procedure (3 h), biomass loadings in the range of 100–200 g L−1 are selectively delignified in 10 min at 150 °C by using choline chloride:formic acid DES (1:2 molar ratio), rendering lignin yields of 60–80% (ca. ~ 40–60 g lignin L−1). Ball milling, microwave irradiation, and DES systems are much more efficient than ball milling, conventional heating, and DES system. The obtained lignins exhibited similar Fourier-transform infrared spectroscopy (FTIR) profile to that of milled wood lignin (MWL), indicating minimal functional group changes.Graphical abstract

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.