Abstract

Herein, we show that we can synergistically optimize the electrical and thermal transport properties of CaMnO3 via doping Sr. All the samples exhibit a single phase with an orthorhombic symmetry within the experimental doping range (0-10%). Sr doping significantly reduces resistivity while maintaining a relatively high absolute value of Seebeck coefficient, resulting in an effective enhancement in the electrical properties of the material. The maximum power factor (∼ 3.01 μ W cm−1 K−2) is achieved at 873 K for Ca0.96Sr0.04MnO3, which is three times larger than that of the un-doped CaMnO3. The thermal conductivity governed by lattice thermal conductivity is notably decreased compared with the un-doped sample, which is mainly attributed to the decreased grain size and large mass and strain fluctuations caused by Sr doping, and the thermal conductivity decreases with increasing Sr doping level. The enhanced power factor and significantly reduced thermal conductivity lead to a maximum ZT value of 0.15 at 873 K in the Ca0.90Sr0.10MnO3 sample, indicating that CaMnO3 is a potential candidate for high-temperature application.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.