Abstract
Bismuth telluride (Bi2Te3) is the only commercial thermoelectric material so far, and it is also the best thermoelectric material with the best performance at room temperature. However, up to now, the zT value of n-type materials used on a large scale is only about 1.0; this makes the thermoelectric conversion efficiency of thermoelectric devices and thermoelectric applications stagnant. Therefore, under the synergistic action of BiI3 and In, the properties of n-type Bi2Te2.7Se0.3 material are improved. The experiments show that BiI3, which is nontoxic and non-absorbent, can effectively improve the power factor of the material and inhibit the bipolar effect and is an effective dopant. After the inclusion of In, due to the low bond energy of the In-Te bond, it is easy to form the InTe phase in the matrix material and then introduce the second phase, and the presence of the second phase in the material will scatter phonons and reduce the lattice thermal conductivity so that it can reach 0.31 W m-1 K-1 at 350 K. Ultimately, a high maximum zT of 1.20 at 325 K and a remarkable average zT of 1.04 (300-500 K) are attained in the In0.005Bi1.995Te2.7Se0.3 + 0.13 wt % BiI3 sample.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.