Abstract
Wood Plastic Composite (WPC) was prepared with simul (soft wood, density = 0.4g/cc) and butylmethacrylate (BMA) monomer using 10% methanol as the swelling agent. Effect of additives including (i) multifunctional acrylates such as tripropylene glycol diacrylate (TPGDA), trimethylol propane triacrylate (TMPTA) (ii) oligomer acrylates like the urethane (UA), epoxy (EA) and polyester (PEA) acrylates and (iii) N-vinyl pyrrolidone (NVP) was investigated using 1 to 3 Mrad dose at 0.8 Mrad/h. Synergistic increases in polymer loading yields was achieved in presence of the additives, particularly with the trifunctional acrylate (TMPTA). In addition, acid as well as urea were also used as co-additives and synergistic enhancement in yields of polymer loading were obtained. The synergistic polymer loading by acid addition causes substantial decrease in tensile strength of the composite; but other additives and co-additives increase both the polymer loading and the tensile strength in these systems.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.