Abstract

The swelling and deswelling of isotropic and oriented polyamide 11 (PA11) with formic acid have been determined as functions of temperature and acid solution concentration. During swelling, dimension relaxation, partial dissolution of crystallites and extraction of low molecular weight chains occur. During deswelling, amorphous chains recrystallize and after complete drying, the original morphology with the same orientation is restored. This memory effect is due to strain-induced crystallization in the PA oriented gel.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.