Abstract

Suspension roasting furnace was used as the reactor of magnetic roasting of fine grained siderite, and the N2 was used as the conveying gas. The results show that, the siderite ore be roasted at the conditions of gas velocity is 1.7m/s, and the roasted time is 12.35s, according to magnetic separation can obtained iron concentrate grade is 65.04%, and recovery rate is 93.03%.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.