Abstract

Microlattices hold significant potential for developing lightweight structures for the aeronautics and astronautics industries. Laser Powder Bed Fusion (LPBF) is an attractive method for producing these structures due to its capacity for achieving high-resolution, intricately designed architectures. However, defects, such as cracks, in the as-printed alloys degrade mechanical properties, particularly tensile strength, and thereby limit their applications. This study examines the effects of microlattice architecture and relative density on crack formation in the as-printed 718 superalloy. Complex microlattice design and higher relative density are more prone to large-scale crack formation. The mechanisms behind these phenomena are discussed. This study reveals that microlattice type and relative density are crucial factors in defect formation in LPBF metallic alloys. The transmission electron microscopy observations show roughly round γ″ precipitates with an average size of 10 nm in the as-printed 718 without heat treatment. This work demonstrates the feasibility of the additive manufacturing of complex microlattices using 718 superalloys towards architectured lightweight structures.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.