We report on the synthesis of two types of Ag nanoparticles (NPs) and the influence of adsorbed surfactant size on the NP surface for surface-enhanced Raman scattering (SERS) signals. Both particles were of similar size and morphology but were covered by surfactants of different sizes; one surfactant was sodium citrate (molecular weight: 258) and the other was sodium polyacrylate (molecular weight: 2100). For SERS measurement, 4-mecapobenzoic acid and 4-naphthalene thiol as Raman-active dyes were immobilized on the surface of each AgNP. The signals from Raman-active dyes on AgNPs covered with citrate displayed 10 times higher intensity than those from polyacrylate-stabilized AgNPs. Elemental analysis (EA) revealed that the average weight percentage of sulfur is 0.94 wt% and 0.12 wt% for citrate-stabilized and polyacrylate-stabilized AgNPs, respectively. The sulfur content difference was attributed to the size of the existing surfactant influencing the ligand exchange by steric hindrance and subsequently the amount of sulfur content of the particles. These experimental results suggest that the size of initial surfactant should be taken into account when synthesizing a metal particle for enhancing SERS signal.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.