Abstract

Molten Soda lime glass (SLG) was penetrated into the surface of ZTA at 1500°C for the holding time of 1 to 10 h. The depth of the glass penetration increased with increasing holding time. The thermal expansion mismatch and elastic property mismatch between the penetrated glass and ZTA produced residual compression in the surface region during cooling. This residual compression enhanced the flexural strength and fracture toughness remarkably.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.