Abstract

To evaluate coating materials regarding color and roughness changes when applied over a composite resin. Specimens were made using Filtek Supreme Ultra. Coating materials were applied over the specimens' surface: Control (CTRL); Adper Single Bond Plus (SB); Scotchbond Universal (US); Clearfil SE (CL); Ambar APS (APS); Bioforty (BF); Fortify (FF); PermaSeal (PS); G-CoatPlus (GC). Specimens were evaluated regarding color changes (∆E00 ) using spectrophotometer (n = 10); surface roughness (Ra), using optical profilometer (n = 10); surface topography, using scanning electron microscopy (n = 1); and thickness of material, using optical microscopy (n = 1). Analyses were made before and after 24, 72, and 168 hours of storage in wine, used as a staining solution. Data was statistically analyzed using analysis of variance, Tukey and Pearson tests (α:.05). None of the materials presented color stability. ∆E00 increased with increasing storage time at red wine, until 72 hours. BF, FF, PS, SB, and CTRL presented the lowest ∆E00 after 24 hours. APS presented the highest ∆E00 (32.59; P < .05). Regarding roughness, initially, surface sealants and APS presented the lowest values. After 168 hours, GC presented the lowest Ra (0.60; P < .05). All the materials presented color and roughness changes after storage in red wine. Some coating materials can be applied over the surface of RBC restorations without changing its color stability or surface roughness.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.