Composite materials used in the prosthetic and orthotic fields have helped improve the fabrication of sockets. Laminated sockets proved to be stronger than conventional thermoplastic sockets. The internal surface of a laminated socket plays an important role in patient comfort and is influenced by the material used to fabricate the socket. This study analyzes the internal surface profile of five different materials, that is, Dacron felt, fiberglass, Perlon stockinette, polyester stockinette, and elastic stockinette. All sockets were fabricated using an acrylic resin mix with hardener powder at a ratio of 100:3. The internal surface of the sockets was tested using the Mitutoyo SurfTest SJ-210 series for 20 trials. The overall Ra values were 2.318, 2.380, 2.682, 2.722, and 3.750 µm for fiberglass, polyester, Perlon, elastic stockinette, and Dacron felt. Dacron felt yielded the lowest Ra value, thus, producing the smoothest internal surface but requiring high skill and the correct technique during the fabrication of a laminated socket. Fiberglass is considered the best material for the internal surface despite not producing the lowest value individually but overall is the lowest and most consistent, indicating that it is easy to use to laminate prosthetic sockets.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.