Abstract
It is suggested that fibre surface per gram of fibre be used as a measure of fibre fineness. An air-flow method of quickly and accu rately measuring this quantity is described. Either high-porosity (.984 < ε < .994) or low-porosity (.665 < ε < .89) wads may be used with proper calibration, though wads of intermediate porosity are avoided. The method is checked against determinations by a microscope, and calibrations for two particular pieces of apparatus are given.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.