Abstract
In order to investigate the wear behavior of induction-heated 13Cr-2Ni-2Mo stainless steel, we performed the rolling contact fatigue (RCF) tests in water. We interrupted the RCF test at each 1.0×105 cycles and measure the wear loss and observed the contact surface. After the RCF tests, we found the oxygen concentration area in the contact area.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.