Abstract

Hot filament chemical vapor deposition (CVD) technique has been used to deposit diamond films on silicon substrate. In the present study, diamond films were grown at various vol.% CH 4 in H 2 from 0.5% to 3.5%, at substrate temperature and pressure of 850 °C and 80 torr, respectively. Scanning electron microscopy, X-ray diffraction and Raman spectroscopy were employed to analyze the properties of deposited films. The formation of methyl radicals as a function of vol.% CH 4 not only changes film morphology but also increase film growth rate. At low, intermediate and high vol.% CH 4, cluster, faceted cubes and pyramidal features growth, were dominant. By increasing vol.% CH 4 from 0.5% to 3.5%, as the growth rate improved from ∼0.25 μm/h to ∼2.0 μm/h. Raman studies features revealed high purity diamond films at intermediate range of vol.% CH 4 and grain density increased by increasing CH 4 concentration. The present study represents experimentally surface morphology, growth rate and quality of diamond films grown in hot filament CVD system at various CH 4 concentrations.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call