Abstract

The reactivity of the surface of calcium hydroxyapatite (CaHAp) and fluorapatite (CaFAp) was tested and compared by grafting the 1-octylphosphonic dichloride (C 8H 17OPCl 2) using a molar ratio x = 2 or 4, x = n(organic)/ n(apatite). Successful synthesis was confirmed by different characterisation techniques such as X-ray powder diffraction patterns, IR spectroscopy, MAS-NMR ( 1H and 31P) and chemical analysis. The difference between their specific surface area (SSA: 57.46 for HAp and 12.09 m 2/g for FAp), the percentage of carbon measured after treatment with (C 8H 17OPCl 2) and the intensities of IR bands attributed to the grafted moiety suggests that the surface of hydroxyapatite is more reactive than that of fluorapatite. The 31P CP-MAS-NMR spectra of treated fluorapatite show a significant change in isotropic signal due to the protonation and deprotonation of superficial phosphate group. This can be explained by the difference in the nature of inorganic material.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.