Abstract

Plastic pellets contain a certain percentage of moisture. During injection molding, the moisture appears as silver streaks on the molded part surface. Therefore, drying operation before molding is an indispensable requirement. This is not only time-consuming but also requires additional energy consumption and cost. This study investigates whether silver streak can be minimized and improved by using gas counter pressure (GCP) to restrict the fountain flow effect in the melt filling process. Effect of GCP values on the silver-streak appearance and the associated surface gross were investigated. The higher the GCP pressure used, the less the silver streaks appeared. When the used GCP pressure reached 50 bar, the silver streaks were no longer seen on the surface, regardless of the moisture content. Moreover, a new monitoring method based on the integral value of the pressure was also built up to assist in plasticizing parameter optimization. Molded parts with a pressure integral value higher than a critical value were no longer troubled by sliver streaks from moisture. This can be a useful way to optimize process parameters when molding moisture contained plastic material.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.