Abstract
In the design of advanced polymeric biomaterials there is a need to tailor the surface chemistry of the biomaterial to elicit beneficial interactions with cells and biomolecules. To facilitate the fabrication of complex biomaterial surfaces, we have previously described the synthesis and application of a poly(lactic acid)−poly(ethylene glycol) block copolymer (PLA−PEG) with the biotinylated PEG end groups (final polymer termed PLA−PEG-biotin). This polymer is biodegradable and resistant to nonspecific protein adsorption, and the biotin moiety allows surface chemical engineering to be achieved using avidin−biotin interactions. Here, we describe a detailed surface analysis of this polymer using X-ray photoelectron spectroscopy and surface plasmon resonance analysis. This analysis has revealed that the avidin−biotin surface engineering strategy is a rapid method of immobilizing biomolecules at biomaterial surfaces under aqueous conditions. The surface engineering generates a specific and high-density change ...
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.