Abstract

The depth of the damaged surface layer and the changes of hysteresis loop caused by surface processing in Mn0.53Zn0.35Fe2.12O4 single crystal are measured. The results obtained are treated as a consequence of the crystal structure deformation at the surface and coherent limited domain wall movement.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.