Abstract

This paper deals with the surface crack growth path description and the fatigue life prediction due to repeated rolling/sliding contact on the elastic half-space, accompanied by frictional heat generation and crack-face pressure. The stress intensity factors are analyzed for the surface crack which is kinked in multiple times from the inclined initial main crack. The rolling/sliding contact is simulated as a Hertzian contact pressure and a frictional load with heat generation, moving with constant velocity over the surface of the half-space. Applying the maximum energy release rate criterion to each kinked angle, the crack growth path can be described, and employing a mixed mode fatigue crack growth law, the associated fatigue life also can be predicted. The effects of frictional coefficient, slide/roll ratio and crack-face pressure on the crack growth path and associated life are considered for a high carbon-chromium bearing steel (SUJ 2).

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.