Abstract

ZnxMg1-xFe2O4 mixed oxide spinels (x=0.0, 0.2, 0.4, 0.6, 0.8, and 1.0) were prepared by conventional solid state reaction method. Bulk and surface characterization of these ferrites were carried out by different techniques. The ratios Zn/Fe and Mg/Fe determined by PIXE and AAS were nearly as expected from the synthesis mixture, i.e. following the substitution model. XRD shows only a spinel structure (fcc) with increasing lattice parameter as x increases from 0 to 1. The bulk ratios of tetrahedral to octahedral sites occupied by Fe cations measured by NGR are in good agreement with the theoretical bulk stoichiometry. LEIS results indicate a Mg substitution by Fe cations at the surface. Only octahedral sites are proposed at the surface. The transition from inverse to normal spinel was follow through NGR-spectra occurring at x=0.4.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.