Abstract

Purpose – This paper aims to find an optimal surface treatment of commonly used polymeric substrates for achieve the high adhesion of printed structures. For this reason, the investigation of substrates surfaces from different perspectives is presented in this paper. Design/methodology/approach – The contact angle measurements as well as the roughness measurements were realised for the analysis of surface properties of investigated substrates. The impact of applied chemical agents for surface treatment onto the wettability is analysed for polyimide, polyethylene terephthalate and polyethylene naphthalene substrates. Findings – The results prove the correlation among wettability, surface energy and work of adhesion with respect to the theoretical background. The surface treatment of polymeric substrates by chemical agents, such as acetone, toluene, ethanol, isopropyl and fluor silane polymer, has a significant impact onto the wettability of substrates which affects the final deposition process of nanoinks. Originality/value – The main benefit of the surfaces’ investigation presented in this paper lays in surface modification by readily available chemical agents for optimising the deposition process nanoinks used in inkjet printing technology.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.