Abstract

This work presents the first corrosion analysis of 4-methyl-2-phenylimidazole (MePhI) corrosion inhibitor for brass immersed in 3 wt.% NaCl solution, wherein MePhI was shown to be highly effective. Moreover, the structure of the surface layer, the formation of an organo-metallic complex, the spatial distribution of MePhI, and the thermal stability of the MePhI surface layer were described in detail using time-of-flight secondary ion mass spectrometry analysis and X-ray photoelectron spectroscopy. Furthermore, a gas cluster ion beam source using different sizes and accelerating energies of the clusters was also employed to slowly sputter the organic surface layer associated with the surface layer analysis.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.