Abstract
Fabrication of fluoride phosphate glass optical fibers using the extrusion method for preform fabrication has been studied using the commercial Schott N‐FK51A glass. The extrusion step was found to create a surface layer of differing composition from the bulk glass material, leading to defects drawn down onto the optical fiber surface during fiber fabrication, resulting in high loss and fragile fibers. Similar phenomena have also been observed in other fluoride‐based glasses. Removal of this surface layer from preforms prior to fiber drawing was shown to improve optical fiber loss from >5 dB/m to 0.5–1.0 dB/m. The removal of this surface layer is therefore necessary to produce low‐loss fluoride phosphate optical fibers.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.