Abstract

ABSTRACTIn this study, nylon 12 (5–25 wt %) was melt blended with a supramolecular thermally repairable thermoplastic elastomer (ATA‐POE), which was generated by crosslinking of maleated polyethylene‐octene elastomer (mPOE) with 3‐amino‐1,2,4‐triazole (ATA), in an internal mixer. The effect of nylon 12 content on the phase morphology, thermomechanical properties, and thermally triggered scratch repairing effects of the ATA‐POE/nylon 12 blends was investigated. Scanning electron microscopy results showed that nylon 12 formed a dispersed phase with submicron scale in a continuous ATA‐POE phase. Fourier transform infrared spectroscopy and differential scanning calorimetry analysis revealed that there are extensive hydrogen bonding interactions between the ATA‐POE and nylon 12 in the blends, which was manifested by a decrease in the melting temperature of each polymer component. Tensile and dynamic mechanical test showed that tensile modulus increased with increasing nylon 12 contents in the blend with maintaining fairly high elastic recoverability. Furthermore, the blends containing up to 20 wt % of nylon 12 showed good scratch repairing effects when they are heated above melting temperature of the ATA‐POE phase in the blend. © 2014 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2015, 132, 41511.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.