MgMn2O4 spinel oxide has a very positive redox potential (2–3 V vs. Mg/Mg2+) and is a promising positive electrode material for Mg rechargeable batteries. However, the charge of MgMn2O4 cannot be adequately accumulated due to oxidative electrolyte decomposition resulting in poor cyclability. We have examined the effect of transition metal ion substitution in Mg spinel oxides and demonstrated that oxidative electrolyte decomposition is suppressed by replacing Mn cations in MgMn2O4 with Fe. Tetragonal MgMn2O4 spinel was converted into cubic-phase Mg(Mn1−xFex)2O4, when 20% or more of its Mn3+ ions were replaced by Fe3+ (x = 0.2, 0.4, 0.6, 0.8, 1). Mixed Mn–Fe cubic spinel oxides exhibited enhanced cyclic performance due to the suppression of oxidative electrolyte decomposition and improved structural stability. This approach provides a means of improving the electrochemical performance of Mg battery systems without requiring thermodynamically stable electrolytes.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.