The secondary relaxation of poly(2-vinylpyridine) (PVPy) in a complex and blends with poly(4-vinylphenol) (PVPh) was studied by broadband dielectric spectroscopy. The polymer complex can be obtained by mixing PVPh and PVPy in methyl ethyl ketone as a result of the very strong hydrogen bonding between two polymers, and it has a glass transition temperature higher than that of either component. The secondary relaxation of PVPy is clearly suppressed in the complex, and it is found that the reduction of its dielectric relaxation strength is approximately proportional to the intermolecular hydrogen bonding fraction. In addition, the relaxation time of unassociated PVPy side groups is also slowed down by about 1 decade compared to that of the neat PVPy. Homogeneous PVPh/PVPy blends can be achieved if the polymers are mixed in N,N-dimethylformamide. However, the degree of intercomponent hydrogen bonding is much lower in the blends, and therefore the suppression of the PVPy secondary relaxation is not as signific...

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.