Abstract

( Co x Pt 1−x ) 1−y Si y alloys with Si content from 1 to 20 at. % have been grown over a range of growth conditions. Co-deposition of even trace amounts of Si with Co–Pt alloys causes the growth-induced magnetic anisotropy and chemical clustering found in these vapor-deposited alloy films to decrease or vanish. It also causes significant reduction in grain size. Addition of 5 at. % Si eliminates anisotropy completely. Addition of 1 at. % Si produces a film with magnetic properties identical to pure Co–Pt alloys grown at lower deposition temperatures. We suggest this suppression of anisotropy and related effects are due to a decrease in surface mobility during growth in the presence of even trace amounts of Si.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.