Abstract

We demonstrated an erbium-doped mode-locked fiber laser using a single-walled carbon nanotube-dispersed polyimide (SWNT-PI) film. Different mode-locking operations were compared and analyzed utilizing SWNT-PI films with different concentrations (2, 1, and 0.25 wt.%, respectively). It was found that the continuous single-pulse mode-locking operation was often accompanied by a continuous wave oscillation part for the 1 and 0.25 wt.% SWNT-PI films, whereas the 2 wt.% SWNT-PI film presented the most excellent mode-locking performance, thanks to sufficient modulation depth. Using the 2 wt.% SWNT-PI film, a stable pulse train with a pulse width of 840 fs and a repetition rate of 15.3 MHz was achieved. The average output power was 0.33 mW at the pump power of 155 mW under an output coupling ratio of 10%. Operational performance of the laser cavity when employing the 2 wt.% SWNT-PI film was also demonstrated.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.