Mo-Si-B alloys consisting of a Mo solid solution and the intermetallic phases Mo{sub 3}Si and Mo{sub 5}SiB{sub 2} were synthesized by mechanical alloying followed by sintering and hot isostatic pressing to field an ultra-fine (triplex) microstructure with all three phases being in the sub-micron range. at temperatures as low as 1300C the material exhibits superplasticity, with tensile strain to failures of 200-400% at strain rates as high as 10{sup -3}s{sup -1}.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.