Abstract

Superplastic deformation behaviour of two aluminium-based AA7XXX type alloys with Sc and Zr additives distinguished by the presence and absence of coarse eutectic Al9FeNi particles are compared. An alloy with Al9FeNi particles exhibits high strain rate superplasticity at constant strain rate range of 5×10−3–8×10−2s−1 with elongation of 915% due to extensive dynamic recrystallisation. Effective activation energy of superplastic deformation, surface relief of deformed samples, and grain structure evolution are analysed. Particle-depleted zones are found in the alloy with Al9FeNi particles at strains higher than 1.25.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.