Abstract
Complex shaped, ultra thin-walled parts can be manufactured using superplastic forming. Hot working temperature for the production of fine-grained billets (d=5-15 μm) out of ATI Allvac 718Plus® superalloy is in the range of 982-1038°C. An ultrafine-grained structure (d=0.3 μm) was produced by multi-axial forging with a gradual decrease of the forging temperature from 950 to 700°C. Superplastic properties of the alloy were carried out in the temperature interval of 700-950°C. It has been revealed that the fine-grained alloy provided superplastic elongations about 300% at 950°C and strain rate of 10-4 s-1. The highest elongation of ultrafine-grained alloy was about 1450% and very low flow stresses were reached at 900°C and strain rate of 3×10-4 s-1. The ultrafine-grained alloy showed superplastic properties also at 700°C (0.62Tm). The microstructure and superplastic properties of the alloys 718 and 718Plus are compared.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.