SuperLig® 644 resin was exposed to simulated Hanford waste solution under air atmosphere or in protated inert environment, and in 0.5M HNO3 solution for 15 days and 45 °C. The degradation was evaluated by cesium batch distribution measurement.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.