Abstract

Studies at Commissariat à l’Energie Atomique (CEA) have been under way for three years in an attempt to find methods for preventing and stopping denting. Tests have been performed in 28 model boilers (Ajax with U tubes and Clarinette with straight tubes). In these boilers, with continuous injection and blowdown, and heat flux is ∼40 W·cm−2 (126 900 Btu/ft2·h). The kinetics of denting has been studied with different levels of faulting. Some high-temperature electrochemical measurements established the mechanism of denting in the boiler tests. Denting kinetics can be rationalized in terms of three main parameters: faulting level, heat flux, and relative mechanical strength of the tube compared to the support plate.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.