In this paper, the slag-metal equilibrium experiments were performed to investigate the effect of TiO2 concentration in the slag and basicity (R=wt%CaO/wt%SiO2) on the sulphur distribution ratio (Ls) between CaO-SiO2-TiO215%Al2O3-8%MgO slag and carbon-saturated iron at 1773 K. Sulphide capacities (Cs) were calculated based on the sulphur distribution ratio. The sulphur distribution ratio and sulphide capacity of CaO-SiO2-TiO2-15%Al2O3-8%MgO stage increase with increase of basicity and with decrease TiO2 concentration in the slag. The relationship between sulphide capacity of CaO-SiO2-TiO2-15%Al2O3-8%MgO slag and optical basicity was also investigted. The experimental results are useful for smelting vanadium titaniferrous magnetite of blast furnace.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.