Abstract
Stainless steels undergo a sharp rise in pitting corrosion rate as the potential, solution concentration, or temperature is changed only slightly. We report experiments using real-time microscopic in situ visualizations that resolve the nucleation and evolution of individual pits during the transition. They suggest that the sudden onset of corrosion is explained by an explosive autocatalytic growth in the number of metastable pits and that stabilization of individual pits takes place only later. This finding agrees with a theoretical approach treating the onset of pitting corrosion as a cooperative critical phenomenon resulting from interactions among metastable pits, and it extends perspectives on the control and prevention of corrosion onset.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.