Abstract

Juxta-articular defects pose significant challenges due to the high risk of fracture of the subchondral plate and articular cartilage. We evaluated the mechanical and histomorphological repair process of caprine subchondral femoral defects augmented with either a bioresorbable in situ setting hydroxyapatite cement (HAC), polymethylmethacrylate (PMMA), autogenous bone graft (AG), or left empty. Twelve-mm subchondral defects were made bilaterally in the medial femoral condyles of skeletally mature goats and augmented with a test material or left empty. Femurs were harvested at varying time periods out to 2 years and evaluated for subchondral stiffness and histomorphological indices. Several defects augmented using autograft or left empty sustained focal fracture of the subchondral plate. No HAC or PMMA augmented defects showed evidence of subchondral fracture. The HAC and PMMA augmented defects showed comparable stiffness at all time points. The mean volume fraction of HAC remaining within the defects progressively decreased from 96% at 24 h to 38% at 2 years. The new bone replacing the HAC appeared to have normal physiological architecture and orientation. In situ setting hydroxyapatite cement may be a viable alternative for the repair of subchondral defects with an important advantage that while undergoing gradual resorption and replacement with host bone, mechanical integrity of the skeletal defect is maintained.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.