Abstract
The mechanical properties of hybrid composite interfaces are critical in determining the overall properties of composite materials. To investigate the mechanical performance of hybrid composite interfaces, an accurate and efficient method must be developed. In this work, nanoindentation is used in this work to investigate the mechanical performance of the carbon/glass interface and the influence of the distance between carbon and the glass fibers on the modulus of the thermoset matrix. The results show that the interface sizes around the carbon and glass fibers are around 1.5 and 2.0 μm, respectively. The modulus around the carbon fibers is 5–11 GPa without the fiber effect, while that around the glass fibers is 4–10 GPa. The modulus of the matrix is not affected by the two types of fibers when the distance between them is greater than 4.5 μm.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.