Abstract

In this study the influence of the content of SKD-B butadiene rubber and BNKS-18 AMN nitrile rubber in the blend on the properties of the resulting elastomers is investigated. The combination of frost-resistant and aggressive media resistant rubbers in the blend allows to adapt the properties of vulcanizates to the required operating conditions. The research revealed that the level of physical and mechanical properties, aggressive media resistance and frost resistance depend on the ratio of rubbers. The study of properties of elastomers revealed two glass transition temperatures and two thermal transitions at negative temperatures corresponding to nitrilebutadiene and butadiene rubbers. The phase morphology of elastomers, characteristic for butadiene nitrile or butadiene rubbers in dependence on their ratio in the blend, was investigated by electron microscopy. Based on the developed elastomer, dust covers for CV-joints were produced. They were tested in real operating conditions in the temperature range from –52 to 33°C.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call