In this study, 1mm thick Fe-Mn-Si shape memory alloy was welded by both sides using YAG laser welding. In a certain range of parameters, the optimal processing parameters for the maximum tensile strength are current 100 A, pulse frequency 3 Hz and pulse width 15 ms by orthogonal experiment. With the optimal processing parameters, the tensile strength of the welded joint can achieve 94% of base material,and the fracture appears in the center of welding seam and the surface morphology of welding seam is good. The influence of processing parameters on tensile strength of weld joint is directly embodied in cross-section of the welding seam morphology. In the laser welding, the tensile strength of nonpenetration in seam and hourglass shape welded joint is generally poor, and the perfect welded joint has conditions such as wide welding seam, deep penetration, weld pool filling and “non-hollow”. Most importantly, the central area in cross-section of the welding seam is the widest.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.