170P1/DX54D+Z was a kind of laser-welding-tailored-blanks with unequal thickness. But it usually occurred poor welding seam especially when the thickness has an obvious difference. In this study, it was explored that the important influence factors of welding seam and formations based on the micro-hardness, microstructure testing and cupping experiment. The micro-hardness and microstructure of base metal,welding seam and heat affected zone (HAZ) has been observed. In addition, offset of welding seam and Erickson value was also measured. It was analyzed that the effect of the thickness difference and chemical compositions on welding seam and formation. It was stated that there were a great influence of thickness difference and chemical compositions on the properties of welding seam and formation.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.