Abstract

FeS solid lubrication duplex layer was prepared on the surface of 45 steel by ion nitrocarburizing and ion sulphurizing process. The sulphide grains in micron and nano scale and holes distributing equably on the duplex layer. The duplex layer is composed of FeS, FeS2 and Fe3N. Under liquid paraffin oil with 0.2wt%n-Fe3O4 lubricating, the synergistic effect between n-Fe3O4 and the duplex layer is produced, and the chemical reaction films including sulphide, sulphate and nitride is formed, which makes the friction factor of the duplex layer keep being the lowest and about 0.075, and the volume loss is reduced by 91% than that of the plain surface, and reduced by 89% and 21% than that of the sulphurized surface and the nitrocarburized surface, respectively.