Abstract

The Polyamide Polyamine Epichlorhydrin Resin was obtained by using adipic acid, diethylene triamine and epoxy chloropropane as raw materials. The factors that would affect the properties of PAE resin were considered, including the reaction time, the dosage of the epoxy chloropropane, the injection time of epoxy chloropropane and the soaking time, and the wet strengthening property of PAE resin were studied through experiments. The results are as following: the ratio of epoxy chloropropane to diethylenetriamine is 1:1, the injection time of epoxy chloropropane is 8.5 min, the reaction temperature is 75 °C and the soaking time is 35min~40min. Under the optimum conditions, the PAE has a higher wet-strength and solid content, and its viscosity up to 25~35cp.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.