Abstract

Microporous Poly (vinyl chloride) (PVC) was prepared by foaming of PVC powders using the solution of 2, 2’-azo-bis-iso-butyronitrile (AIBN) in co-solvent of butanone and cyclohexanone when heated. The effect of composition of solvent and quantity fraction of AIBN also preferred dioctyl phthalate (DOP) on the structure of microporous PVC is discussed. The results indicated that much microporosity with average size of 0.2-2μm can be generated when acetone is selected as solvent, 2% DOP and 10% AIBN are used. The microporous PVC is a potential desirable reactor to prepare CaCO3 nanoparticle.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.