Si, Al, Fe were leached from coal gangue to prepare Poly-silicate-aluminum-ferric (PSiAF) coagulant. The optimal technology of preparation of PSiAF was explored through single factor experiment and orthogonal experiment. The effect factor of preparation, such as the content of silica, the molar ratio of Al to Fe (nAl:nFe), the molar ratio of metal (Al+Fe) to Si (nAl+Fe : nSi), the pH of the solution of sodium silicate, were investigated. Results show that The optimal preparation technology were the content of silica of 4%, Al/Fe molar ratio of 1:2, (Al+Fe)/Si molar ratio is 1:1 and pH of 5 of the solution of sodium silicate.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.