Abstract

Abstract In this study, birch xylan was deposited onto elementally chlorine free (ECF) bleached eucalyptus kraft pulp, and the corresponding changes in physical properties were determined. An aqueous 5% birch xylan solution at pH 9 was added to 5 wt% slurry of bleached kraft eucalyptus fibers, with stirring at 70 °C for 15 min after which the pH was adjusted to 5–6. The xylan enriched fibers were isolated by filtration and used for physical testing. A 1.15 wt% adsorption of birch xylan on the kraft fibers at 8% xylan addition increased the tensile index, strain and tensile energy absorption values by ∼10%, while the burst index increased by 20.15%. The tear index increased by 2.55% with the adsorption of 0.87 wt% birch xylan on the eucalyptus kraft pulp at 3% xylan addition. The pulp beatability was also improved by adding birch xylan. The surface morphology of the unmodified and modified pulp samples were analyzed using atomic force microscopy (AFM) in the tapping mode. The analysis revealed the differences in the fine structure of fibers which showed micrometer-sized xylan structures spreading over the fiber surfaces.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.