Abstract
In order to reveal the formation mechanism in PAN wet-spinning process, the Magnifying Method was used to determine the mass transfer rate difference between solvent and coagulant by measuring the weight loss percent of the spinning dope at different interval in the coagulation bath. Then the effect of coagulation condition on and on structure and properties of as-spun fibers was discussed. It was found that increased along with hoist of the molecular volume of coagulants or the coagulation bath temperature but decreased with the increase of the dope solid content or coagulation bath concentration. When the coagulation condition was very moderate(high solid content, low bath temperature or high bath concentration), the was smaller, the counter-diffusion took place slowly and peacefully, and sequentially an even and compact meshwork microstructure was obtained, thus the density and breaking tenacity of as-spun fibers increased gradually.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.