Abstract

Through study on the regulation of tensile strength and reduction of area after artificial aging and natural aging for SWRH82B wire rod, indicate that the tensile strength of wire rod unchanged through artificial aging or natural aging treatment while the reduction of area changes significantly the reduction of area is effected by aging temperature and aging time. Reduce the residual stress in the wire rod and lattice distortion is the main reason for reduction of area improving the composite brittle inclusions in the wire rod are not good for the rod plastic recovery.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.