Abstract

In order to further improve the filtration performance of glass fiber filter material, the surface of glass fiber filter material was modified by preparation of nano-SiO2 and polytetrafluoroethylene (PTFE) emulsion compound finishing solution, and the permeability and filtration efficiency of the filter material before and after modification were tested. The results show that the filtration performance of the filter material is improved after surface modification. The content of SiO2 is 0.8g, the mass fraction of PTFE is 5%, the finishing time is 6h, the filtration efficiency of the modified filter material is 64.67%. At this time, the quality factor is the maximum, and meet the requirements of high efficiency and low resistance.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.