The effect of Ni/Co ratio on the catalytic performance of NiCo/ceramic foam catalyst for hydrogen production by steam reforming of real coal tar was studied. The NiCo/ceramic foam catalyst was synthesized by deposition-precipitation (DP) method and characterized with different methods. The experiments were conducted in a two-stage fixed-bed reactor. The results showed that the reducibility of the metallic oxides in bimetallic NiCo/ceramic foam catalysts was influenced obviously by the Ni/Co ratio.Both gas and hydrogen yield increased first and then decreased with the decline of Ni/Co ratio, and the highest hydrogen yield of 31.46 mmol g−1 was obtained when the Ni/Co ratio was 5/5. The lowest coke deposition of 0.34 wt% was generated at the same Ni/Co ratio. The lifetime test showed the catalyst maintained catalytic activity after 14 cycles (28 h), indicating the coal tar steam reforming on NiCo/ceramic foam catalyst is a promising method for hydrogen production.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.